FAA Advisory Circular 43.13-1B

Acceptable Methods, Techniques, and Practices

Aircraft Inspection and Repair

AC 43.13-1B | 2. Fabric Covering | 2. Application of Dope | 2-23. Coating Application Defects

Previous
Next
9/8/98
AC 43.13-1B
(1) Spray gun not properly adjusted to
(4) Viscosity of material being sprayed
spray a wet, smooth surface.
is too high.
(2) Overspray on a partially-dried sur­
face.
(3) Spray pattern not sufficiently over­
lapped on each pass.
(5) Metallic finishes sprayed too heav­
ily allowing metallic pigments to move or flow
after deposit, causing a marbled appearance.
2-24.2-29. [RESERVED.]